u.p. hobagama first firing part 4 and firebox rebuild

updated thu 9 sep 10

 

gary navarre on tue 7 sep 10


OK Folks, (guess I'll do like the message said and re-post with changes)

Here's a little more video of slowly heating the moisture out of the kiln..=
.

http://www.youtube.com/watch?v=3Dj7dzNwZ2YOs

... without much smoke yet but that will change later. The pace should star=
t to pick up soon so stay tuned for more as I continue to edit what I shot.

I'm also still in the middle of rebuilding the firebox with some decent pro=
gress at the bottom of this Fotki page...

http://public.fotki.com/GindaUP/ca/kpap/uphwfkl3/

I've decided to start adding some soap sized primary air holes lower down i=
n the walls of the Bourry box closer to the hobs and the combustion zone. D=
uring the last firing Rick commented on the "Dragon Tongues" of flame risin=
g up into the top of the Bourry and that the draft should be pulling that h=
eat down into the chamber. I realized the fuel was looking for air coming i=
n the holes along the top. If I add more holes closer to the zone of combus=
tion lower down the walls I think I can prevent that air hungry back lickin=
g of flame up inside the Bourry to the primary air ports even though it loo=
ks cool when it's at high temperature with flames belching out all orifices=
. There is a good shot of that in the second firing videos but we will get =
to that later so enjoy and stay in there eh.

Gary Navarre
Navarre Pottery
Navarre Enterprises
Norway, Michigan, USA
http://www.youtube.com/GindaUP
http://public.fotki.com/GindaUP/