gary navarre on fri 13 aug 10


Hey Folks,

I decided to keep going with the ideas I've had for increasing the volume =
and shape of my Bourry box so it will spread the fuel better and get more a=
ir under the fuel in the Pignose and Bourry mouse holes...

http://public.fotki.com/GindaUP/ca/kpap/uphwfkl3/new-mousehole-covers-jpg.h=
tml

(click picture or next for results or previous for setup)

My thinking is the air coming in gets heated on the way and expands in vol=
ume two or three times at the coal pile. Let us now pray the warped shelf s=
tays in one piece. I can also see something of the step firebox in the mous=
e hole profiles with a long tread and short riser. This should work just as=
good so stay in there eh.

Gary Navarre
Navarre Pottery
Navarre Enterprises
Norway, Michigan, USA
http://www.youtube.com/GindaUP
http://public.fotki.com/GindaUP/