pulverizing recycled kiln lag

updated sun 1 aug 10

 

gary navarre on sat 31 jul 10


Hey Folks,

Since I decided to adjust how the firebox is built I needed a way to crush=
the semi-fired lag back into a useable mix for when I put the bricks back =
together...

http://public.fotki.com/GindaUP/ca/cam/prkl/

The inspiration came from watching the African chicks an public TV poundin=
g Millet in a stump with a chunk of wood log so I figured I could have a go=
. I could pound for 15-30 minutes or so at a time and in about 3 or 4 days =
now have 125lbs. of new lag powder and got some upper body workout to boot.=
Don't need to get better than that but it probably will so stay in there e=
h.

Gary Navarre
Navarre Pottery
Navarre Enterprises
Norway, Michigan, USA
http://www.youtube.com/GindaUP
http://public.fotki.com/GindaUP/