h20 for a clay body

updated mon 21 jun 10

 

Jon Pacini on sat 19 jun 10


Greetings All ---Hi Randall----20% water is a good rule of thumb---

Best regards
Jon Pacini
Clay Manager
Laguna Clay Co

----on vacation and making pots in beautiful Christmas Florida

Michael Wendt on sat 19 jun 10


When I mix the Helmer body, I use 300 LBS of dry ingredients
to 80 LBS of water and weigh out the ingredients very
accurately.
Regards,
Michael Wendt