lili krakowski on thu 25 mar 10


I truly am too hectic right now to check out the exact figures. =3D
However.

The carbonate is about half the "stength" of the oxide. Therefore one =3D
should use about twice as much.

However again the effect is probably NOT identical, as the carbonate =3D
disperses better, and gives off more gases.

Best solution: test. I would dry out a small batch, then do a straight =3D
line blend and see what is closest to my original.

Lili Krakowski