artist demo times - nceca amaco/brent booth #310

updated fri 12 mar 10

 

Faris, Diana on thu 11 mar 10


Hello All,

In response to a request for booth demo times, please see the following
list of demos and stop by our AMACO/Brent Booths (#310-311):

Artist Demo Times - NCECA

=3D20

Wednesday March 31st

Throwing on a Wheel -

8:30am to 5:00pm - Danny Meisinger=3D20

10:00am to 12:00pm - Mark Issenberg

12:00pm to 3:00pm - Cathy Broski

3:00pm to 5:00pm - Mark Issenberg

=3D20

Glaze Demonstrations -=3D20

9:00am to 10:30am - Linda Arbuckle

1:00pm to 3:00pm - Paul Wandless

=3D20

Thursday April 1st

Throwing on a Wheel -

9:00am to 5:00pm - Danny Meisinger

9:00am to 11:00am - Nan Rothwell

11:00am to 2:00pm - Cathy Broski

2:00pm to 5:00pm - Mark Issenberg

=3D20

Glaze Demonstrations -=3D20

1:00pm to 3:00pm - Paul Wandless

=3D20

Friday April 2nd

Throwing on a Wheel -

9:00am to 4:00pm - Danny Meisinger

9:00am to 11:00am - Nan Rothwell

12:00pm to 3:00pm - Mark Issenberg

=3D20

Glaze Demonstrations -=3D20

1:00pm to 3:00pm - Paul Wandless

=3D20

Diana Faris

AMACO Brent

Tel (800)925-5195 x1302

www.amaco.com

=3D20

Veena Raghavan on thu 11 mar 10


Hi Diana,

Thank you so much for posting the demo program at the AMACO/Brent Booth.
This is so helpful. I am the one who made the request, and I appreciate you=
r
posting the names of the demonstrators and times of the demos. I wish other
vendors would do the same.

I will definitely be at some of the demos.

Thanks again.

Veena