Dean on tue 23 feb 10

Thanks for the replies, I finessed a test firing in a friends mini kiln so =
I'll get to try it out. I've got $1500+ worth of colored clay pots waiting =
to be fired by the end of the week, hence my concern. My old clear was over=
loaded with Gerstley Borate and bleached out my green clay, a terrible reci=
pe. I'll be using this glaze very thin so I hope that this one will be OK.