search  current discussion  categories  glazes - traditional iron glazes 

malcolm davis and shino

updated wed 10 feb 10

 

Liz Willoughby on tue 9 feb 10


Dear All,
I just pulled up the shino show
http://www.clayartcenter.org/v/vspfiles/assets/images/slides/shino%20redux%=
202010/shino%20redux%202010/index.html
that Malcolm curated. Wonderful eye candy for those who have fallen
in love with the shino glaze. It is so interesting how shino can
look so differently on peoples pots, all to do with glaze recipe,
clay used, application, and firing methods. Lots of clayarters
represented, nice to see. Malcolm you did good.
Liz Willoughby in Brighton/Grafton, Ontario, Canada

John Britt on tue 9 feb 10


Here is one you might like!


http://ncclayclub.blogspot.com



John Britt
www.johnbrittpottery.com