favorite porcelain? -not b mix

updated sun 31 jan 10

 

Dean on sat 30 jan 10


In my shrink tests B mix shrank 14% which is a lot and it's not that white.=
=3D
My shrink tests did not agree with Laguna's posted numbers. For instance, =
=3D
they list Dave's and B mix as=3DA0 about 13% and I got 10.5% for Dave's and=
1=3D
4% for B mix.=3DA0 That agrees with my experience, I've had a lot more prob=
le=3D
ms with handles cracking off cups made with B mix than any other clay and r=
=3D
elatively few problems with Dave's. I'll check out Nara,
Mahalos,
Dean

=3D
?
It fires white in oxidation, takes color well, and is less expensive
than Coleman.>