search  current discussion  categories  materials - misc 

other wax option

updated tue 26 jan 10

 

Rikki Gill on mon 25 jan 10


Hi All,

I do a lot of things differently from almost every one else, because I =3D
am mostly self taught.

I hate the smell of hot wax, partly because I know it isn't good for =3D
your lungs. What I do is use Aftosa liquid wax and a small sponge stick.
You can get the sponge stick at all paint stores for about $0.80.
The wax goes on quickly and smoothly, and is dry within minutes. It =3D
lleave a totally clean line.
If you are doing at least a board or few at a time there is no down time =
=3D
waiting for things to dry. This really works better for me than hot wax.

Best,

Rikki Gill
rikigil@sbcglobal.net
www.rikkigillceramics.com