Dearest reader I am looking for glaze recipes for cone6 firings. I'm
new to this type of firing and would love to hear from folks. Possible
suggestions of where to look for recipes would be helpful thanks,Harold





_________________________________________________________
DO YOU YAHOO!?
Get your free @yahoo.com address at http://mail.yahoo.com

Helllll on wed 17 dec 97

>Dearest reader I am looking for glaze recipes for cone6 firings.

Hello Harold.....

here are some web sites you should check out...

http://apple.sdsu.edu/ceramicsweb/ceramicsweb.html

the above is Ceramics Web..... and has two searchable data bases .

also you should check out.....for some tech. type info....

http://www.ceramicsoftware.com/education/glaze/cone6.htm
..

here are some other glaze sites...

http://www.cclay.com/glazes.htm
http://ceramics.miningco.com/blglazes.htm
http://www.whistlepig.com/claytimes/stains.htm