new blue

updated tue 1 dec 09

 

John Britt on mon 30 nov 09


Thought someone might be interested in this new blue pigment that=3D20
was created by accident. Not ready for prime time, but interesting=3D20
nontheless.=3D20

In case you are interested and haven't seen it already, here's a link to=3D=
20=3D

an interesting article.

http://www.nytimes.com/2009/11/24/science/24obpigment.html?
ref=3D3Dscience

John Britt