I do all my lids glazed entirely. Lid and pot are fired separately in the g=
laze
firing. How do you figure out if pot and lid will fit together well when
they are done? I have found that if they fit together well, all glazed and
ready to fire, that they will fit when they come out of the kiln. If they =
fit tightly
unfired they won't fit well when fired. Makes sense........

Eleanora





>Dear Deborah,
>
>Are the lips of the mugs glazed? I've thrown lidded mugs but always leave
>the very top of the lip unglazed so I can fire with the lid on. Some peop=
le
>don't like that, so I've been thinking about firing them separately and
>hoping they still fit together.

--