glaze dots

updated sun 15 nov 09

 

Loren JOnes on sat 14 nov 09


Spritzing the pot is an excellent idea! I love Steven Hills glazes I dont h=
ave access to a spray booth anymore so I am trying to work in another direc=
tion. I will still spray a few pots here and there but not so many. Thanks =
for your kind comments on my work. You were doubley lucky to get Steve and =
Matt, he's another favorite of mine. Peace, Loren




________________________________
From: Mike Gordon
To: Loren JOnes
Sent: Sat, November 14, 2009 2:01:59 PM
Subject: glaze dots

HI Loren,
I can see the Steven Hill influence, your glazes are beautiful! I attended =
a workshop here in Walnut Creek, Ca. that Steven did with Matt Long, they w=
ere great together. I dip my glazes not spray them, the layering makes some=
glazes really sing. You might try putting the dots on while the other glaz=
e is still damp, it sounds like a difference in shrinking rates. Or spray t=
he surface with water first then apply the dots. Mike Gordon