Dennis Gerasimov on sun 13 sep 09


Anyone can recommend a place that has or can make a replacement element
for Sno Industries P-22 kiln?
Thanks!
Dennis

Donald Burroughs on tue 15 sep 09


Hello Denis

Talk to Stan Horton at http://kilnelements.com/. Stan is a great person t=
=3D
o=3D20
deal with and very knowledgeable. Hand makes the element all you have to =
=3D
do=3D20
is in Stan's own words "Tell us the ohms, and gage, and we can make any=3D2=
0=3D

element out of 13,14,15,or 16 gage wire." Since your kiln is not well kno=
=3D
wn=3D20
brand he will also probably need the length of an element. Price is very=3D=
20=3D

reasonable based on the service.=3D20

Regards,
Donald Burroughs

On the web @ http://members.shaw.ca/clayartz