the best thing about a pug mill

updated mon 14 sep 09

 

mel jacobson on sun 13 sep 09


i just did it about twenty minutes ago.

ran a batch of clay out that my apprentice mixed yesterday.

i cannot throw stiff clay any longer.
i added a cup of water, ran it through again.
now it is perfect.
many bags of clay for me are far too hard.
so.
they go in the pug mill.
mel