cprart on mon 8 dec 97





I have a wonderful Cone six glaze that I would like to lower to a cone 4
glaze so it would be compatable with another cone 4 glaze that I have. I
know
nothing about this and was wondering if some of you experts could help me
out. The glaze is

whiting 15
Neph. Syn. 40
Flint 38
EPK 7

I add Cobalt Carb. to make a nice cobalt blue.
Thanks to all--Happy Holidays to all and may it be a safe and happy one.