Bill Merrill on wed 9 sep 09


I forgot to mention that Barnard clay can be used at lower temperatures =3D
in both atmospheres. Carlton Ball told me at a Wyoming Artist =3D
Association that if you used it in lower fire add frit to it. =3D20
He used about 10% frit to a measured amount of Barnard. The outcome was =
=3D
a little rough compared to stoneware....just try it....it may work for =3D
you.
=3D20
Bill