Just to save anyone some time and expense, I would like to add that I have
used the same bats for 25 years without ever sealing the edges or backs
with anything and have experienced no problems. Small and medium sizes are
stacked flat when not in use; larger ones (16"+) and up are stored on edge.

Cheers,
Karen
Yellow Branch Pottery
Robbinsville, NC





>----------------------------Original message----------------------------
>>----------------------------Original message----------------------------

.. We sealed the edges and
>all exposed (chip-board) backs with several coats of Varathane ( clear poly
>urathane sealant )