Byron Temple Orange
Custer Feldspar 49
Cornwall Stone 18
Whiting 18
EPK 6
Ball Clay 9
Red Iron Oxide 6
Zinc Oxide 3
Rutile 4

Gene Arnold wrote:
> Does anyone have the recipe for Byron Temple Orange for cone10 reduction.
> I would like to give it a try but can't seem to find the recipe.

--