bringle slip bubbles

updated wed 29 jul 09

 

jim wightman on mon 27 jul 09


Hello,

I've been using Cynthia Bringle's Slip, brushing it on my pots and have had
no problems with it. Recently I tried dipping my pots and I've had trouble
with bubbles in the slip which makes for an unattractive surface. Does
anyone have an idea how to fix it?

I'm also looking for a clear cone 6 glaze to put over slip, underglaze and
engobes (preferably one without Gerstley Borate).

Thanks for your help!

Karen Nakakihara