how to build a cheap but effective spraybooth

updated sun 16 nov 08

 

Richard Aerni on fri 14 nov 08


Hi all,
Google analytics is a wonderful tool...
When I went to check on what people were looking for when they googled my
website, building a spraybooth came up a number of times. Not sure who is
checking, but if some of you on clayart are interested, I have just added a
couple of postings on my blog (see below) which include pictures and
commentary on how I built mine. I pot full-time, and spray all of my
glazes. This booth, or a variation of the above, has served me very well
for over 20 years. Took me one day to build, and cost maybe $125.
You might want to check it out if you are interested.