search  current discussion  categories  wanted/for sale - wanted 

looking for speckled blue cone 9-10 reduction

updated mon 8 sep 08

 

Sandi Taylor on sat 6 sep 08


Hi Everyone,
I did a test this past summer and the results were nice. For the life of =
me I cannot find the glaze recipe. Does anyone have a glaze they would =
share with me called Speckled Blue cone 9-10 reduction. I would =
appreciate it very much.
One of my pottery buddies is nagging me to find it.
Thanks=20
Sandi Taylor

Angela Davis on sun 7 sep 08


Here's one I've wanted to try, if you do how about a report.

Blue Speckle
Cone 10
Oxidation or Reduction
Potash Feldspar 55
Whiting 15
Ball Clay 5
Silica 200# 25
Red Iron Oxide 4
Rutile Flour 3

Angela Davis

With an eye to the sky In Homosassa


----- Original Message -----
From: "Sandi Taylor"
To:
Sent: Saturday, September 06, 2008 11:28 PM
Subject: looking for speckled blue cone 9-10 reduction


Hi Everyone,
I did a test this past summer and the results were nice. For the life of me
I cannot find the glaze recipe. Does anyone have a glaze they would share
with me called Speckled Blue cone 9-10 reduction. I would appreciate it very
much.
One of my pottery buddies is nagging me to find it.
Thanks
Sandi Taylor

Victoria E. Hamilton on sun 7 sep 08


Hi Angela -

Is this sort of a robins egg blue with speckles? If so, you might contact
Don Sprague in Oregon. He used to have a lovely glaze like this that he
shared with me years ago. I don't have it any more, dang!

Good luck.

Vicki Hamilton
Millennia Antica Pottery
Seattle, WA

-----Original Message-----
From: Clayart [mailto:CLAYART@LSV.CERAMICS.ORG] On Behalf Of Angela Davis
Sent: Sunday, September 07, 2008 7:08 AM
To: CLAYART@LSV.CERAMICS.ORG
Subject: Re: looking for speckled blue cone 9-10 reduction

Here's one I've wanted to try, if you do how about a report.

Blue Speckle
Cone 10
Oxidation or Reduction
Potash Feldspar 55
Whiting 15
Ball Clay 5
Silica 200# 25
Red Iron Oxide 4
Rutile Flour 3

Angela Davis

With an eye to the sky In Homosassa


----- Original Message -----
From: "Sandi Taylor"
To:
Sent: Saturday, September 06, 2008 11:28 PM
Subject: looking for speckled blue cone 9-10 reduction


Hi Everyone,
I did a test this past summer and the results were nice. For the life of me
I cannot find the glaze recipe. Does anyone have a glaze they would share
with me called Speckled Blue cone 9-10 reduction. I would appreciate it very
much.
One of my pottery buddies is nagging me to find it.
Thanks
Sandi Taylor

Sandi Taylor on sun 7 sep 08


----- Original Message -----
From: "Angela Davis"
To:
Sent: Sunday, September 07, 2008 10:08 AM
Subject: Re: looking for speckled blue cone 9-10 reduction


> Here's one I've wanted to try, if you do how about a report.
>
> Blue Speckle
> Cone 10
> Oxidation or Reduction
> Potash Feldspar 55
> Whiting 15
> Ball Clay 5
> Silica 200# 25
> Red Iron Oxide 4
> Rutile Flour 3
>
> Angela Davis
>
> With an eye to the sky In Homosassa
>
>
> ----- Original Message -----
> From: "Sandi Taylor"
> To:
> Sent: Saturday, September 06, 2008 11:28 PM
> Subject: looking for speckled blue cone 9-10 reduction
>
>
> Hi Everyone,
> I did a test this past summer and the results were nice. For the life of
> me
> I cannot find the glaze recipe. Does anyone have a glaze they would share
> with me called Speckled Blue cone 9-10 reduction. I would appreciate it
> very
> much.
> One of my pottery buddies is nagging me to find it.
> Thanks
> Sandi Taylor

Sandi Taylor on sun 7 sep 08


HI Everyone,
Of course we will test this one. I will let you know how it turns out.
Thanks so much.
Sandi Taylor Advanced Student
Manatee Community College
Bradenton,Florida.
----- Original Message -----
From: "Angela Davis"
To:
Sent: Sunday, September 07, 2008 10:08 AM
Subject: Re: looking for speckled blue cone 9-10 reduction


> Here's one I've wanted to try, if you do how about a report.
>
> Blue Speckle
> Cone 10
> Oxidation or Reduction
> Potash Feldspar 55
> Whiting 15
> Ball Clay 5
> Silica 200# 25
> Red Iron Oxide 4
> Rutile Flour 3
>
> Angela Davis
>
> With an eye to the sky In Homosassa
>
>
> ----- Original Message -----
> From: "Sandi Taylor"
> To:
> Sent: Saturday, September 06, 2008 11:28 PM
> Subject: looking for speckled blue cone 9-10 reduction
>
>
> Hi Everyone,
> I did a test this past summer and the results were nice. For the life of
> me
> I cannot find the glaze recipe. Does anyone have a glaze they would share
> with me called Speckled Blue cone 9-10 reduction. I would appreciate it
> very
> much.
> One of my pottery buddies is nagging me to find it.
> Thanks
> Sandi Taylor