which oxide or stain for golden wash?

updated mon 11 aug 08

 

judy smith on sat 9 aug 08


I want to put a light wash of a golden color over a B-mix white clay.=A0 Ca=
n you tell me which oxide or mason stain will give me this color.=0AThanks,=
=0AJudy Smith=0ANashville, TN

Victoria E. Hamilton on sat 9 aug 08


You could try a wash of rutile.

Vicki Hamilton
Seattle, WA=20

-----Original Message-----
From: Clayart [mailto:CLAYART@LSV.CERAMICS.ORG] On Behalf Of judy smith
Sent: Saturday, August 09, 2008 5:49 AM
To: CLAYART@LSV.CERAMICS.ORG
Subject: Which oxide or stain for golden wash?

I want to put a light wash of a golden color over a B-mix white clay.=A0 =
Can
you tell me which oxide or mason stain will give me this color.
Thanks,
Judy Smith
Nashville, TN

Karin Givon on sun 10 aug 08


I've a couple of questions: do you want to glaze this pot? DO you
want the color in the glaze, or do you envision it under a clear ( or
translucent) or over it? What ^ will you fire to, as some B-mix goes
to 5 and some to 10....
You can put a mason stain into your glaze, or make a water/stain
mixture and brush or sponge or spray it on. You should use, I think,
at least 3-5% so it doesn't disappear.
On Aug 9, 2008, at 5:49 AM, judy smith wrote:

I want to put a light wash of a golden color over a B-mix white
clay. Can you tell me which oxide or mason stain will give me this
color.
Thanks,
Judy Smith
Nashville, TN