PSH on mon 24 nov 97

> If anyone has any ideas I would really appreciate them
> Toni M in Durban,

Hello Toni,
Probably a burnt out element, switch or wire.
Regarding checking with your meter. It is a good idea to disconnect one
of the wires going to the elements before doing a reading. This will
guarantee that you are not reading `back through the switch`.
Try this & feel free to call me for assistance if this does not help.
Chris @ PSH 800-465-8544 Canada, 800-296-5456 USA
--