Sally Guger on tue 10 jun 08


Hi all, I haven't tried this glaze even though I use many from Ron and John's book. But I did bump into a nice white satin matt cone 6 glaze about a year ago. I mixed a test amount, then a larger batch- it behaved very nicely. I haven't used it since because it isn't a look that I'm after but here's where I found it. Sally.

(Maybe this is a Clayarter, I don't know!)

http://www.nanhamilton.com/howtodesign/painting/painting.html