I would love to know how can I do bloating where and when I want
I am mostly making beads; I am using cone 6 commercial porcelain clays
colourful Chinese low fire glazes
First I fire to cone six ;glazed beads (not 06 and not bisquing) than I put more glazes usually different colour where it was not enough glaze or if the glaze pulled away or if I do not like it
If I like the bead as it is; I keep it.
Sometime some of the beads come out really ugly I hit it with the dremel tool sander and it comes up interesting connecting holes on the surface
That what I would love to make , but when and where I want
Any ideas?
Thanks Vera

var callCount = 0; function rmvScroll( msg ) { if ( ++callCount > 10 ) { msg.style.visibility = "visible"; } if ( callCount msg.clientHeight ) { newHeight = msg.scrollHeight + delta; } delta = msg.offsetWidth - msg.clientWidth; delta = ( isNaN( delta )? 1 : delta + 1 ); if ( msg.scrollWidth > msg.clientWidth ) { newWidth = msg.scrollWidth + delta; } msg.style.overflow = "visible"; msg.style.visibility = "visible"; if ( newWidth > 0 || newHeight > 0 ) { var ssxyzzy = document.getElementById( "ssxyzzy" ); var cssAttribs = ['#' + msg.id + '{']; if ( newWidth > 0 ) cssAttribs.push( 'width:' + newWidth + 'px;' ); if ( newHeight > 0 ) cssAttribs.push( ' height:' + newHeight + 'px;' ); cssAttribs.push( '}' ); try { ssxyzzy.sheet.deleteRule( 0 ); ssxyzzy.sheet.insertRule( cssAttribs.join(""), 0 ); } catch( e ){} } } function imgsDone( msg ) // for Firefox, we need to scan for images that haven't set their width yet { var imgList =
msg.getElementsByTagName( "IMG" ); var len = ((imgList == null)? 0 : imgList.length); for ( var i = 0; i

Arnold Howard on mon 28 apr 08


From: "VERA ROMODA"
> I would love to know how can I do bloating where and when
> I want

Fast firing is one way to get bloating. I experimented with
self-supporting witness cones inside the Paragon QuikFire
kiln, which reaches 1200 degrees F in about 10 minutes. The
cones did not bend; they bloated.

Sincerely,

Arnold Howard
Paragon Industries, L.P., Mesquite, Texas USA
ahoward@paragonweb.com / www.paragonweb.com