Copper flash on table ware...not raku...but a bright copper flash all the same.
I was post reducing some crystal glaze pots for a friend and tossed in a
few poorly developed copper red pots from previous electric reduction
firings.One in particular got bite bad by a flash of pure copper.
http://www.puttgarden.com/crystal/2008/4-21-08/tn-DSC01253.jpg
All the other experimental pots got flashed but not as dramatic as this one.