>I have two questions; one local and the other general.
> I've been using paper clay and get them dried without much
>warping but when I fire them [lying flat], I get an inordinate amount of
>cracking;


This might be an all too obvious answer but , I do paper
thin porcelain plaques ( not paper clay though ) and fire
them flat on my shelves
with a thin sprinkle of alumina hydrate powder on the shelf ..
The porcelain rolls on that as it shrinks..

Marci Blattenberger