Hank,

Trying again on that plate burner. One different thing about the design in
the vast website of publications for the third world !?!?! is the authors
were recommending a mixture of oil and water. dripping the two together
into a trough together flow to the burner plate.

Faster is often better, more turbulence in the kiln space.

So, is stove oil kerosene?

Joe

The link is to the index of that site. there are lots of links to documents
of various kinds on various subjects.


http://sleekfreak.ath.cx:81/3wdev/CD3WD/INDEX.HTM