Deborah Thuman on thu 25 oct 07


What if.....
You took a ^6 tile and put attached it on edge in a ^10 dish. Not a
fancy dish - just a little pinch pot type dish. You could bisque fire,
test out the ^8 glaze on the ^6 tile, and if it turned the ^6 clay into
a melted mess, the mess would be confined in your little ^10 dish under
the tile.

Deb