e book on fractography of ceramics and glasses

updated sat 20 oct 07

 

WJ Seidl on fri 19 oct 07


Someone posed this in sci.materials

NIST has recently published a free ebook on fractography. Fractography
of Ceramics and Glasses (Special Publication 960-16) was written by
George D. Quinn. It is modestly labeled a "practice guide" but
actually is a 537-page book with lots of images. It can be downloaded
as a 31.7Mb Acrobat (.pdf file) at:
http://www.nist.gov/public_affairs/practiceguides/practiceguides.htm

--