search  current discussion  categories  glazes - traditional iron glazes 

flattening foamy shinos

updated wed 5 nov 97

 

Danny Bird on tue 4 nov 97

A few days ago, I suggested one might try flattening their foamy shinos
with isopropyl alcohol, in a spray bottle. I should've mentioned, that
this is a flammable substance, and caution should be exercised with it's
use. DO NOT USE THIS NEAR AN OPEN FLAME.

Birdboy