Russel Fouts on sun 29 jul 07


I didn't think of this while the thread was going on but if you spray
a solution of CMC on the surface, glazed or unglazed, the trailed wax
or glaze won't blob up.

I've been doing this with very find 'needle' bottles using wax
emulsion and glaze.

With practice and a quick hand, you can get pretty thin lines. I'm
not there yet but I've seen it done. ;-)