waterfall brown green

updated tue 17 jul 07

 

John Sankey on mon 16 jul 07


Has anyone figured out the chemistry of the green phase of this
glaze that appears on horizontal surfaces?

Ferro frit 3134 33.5g
Ferro frit 3195 26g
silica 23.5g
OM-4 ball clay 17g
red iron oxide 12.5g
titanium dioxide 1g

No copper, chrome, or anything else like that. I get the same
result with EPK and oxides rebalanced.

--
(Add 'Byrd' to the subject line of your reply to get through my spam filter)