small lowfire woodkiln results

updated sun 29 apr 07

 

Elizabeth Priddy on sat 28 apr 07


http://www.flickr.com/photos/7973282@N03/


Wood kiln results from second firing of my
small low (cone 7) wood kiln.

Ash works low too. It may need a little glaze.

The chamber on the kiln is 18x18x30 of usable space.

It took 5 hours to get to cone 7.

I will add a few pictures of the kiln itself later.


Elizabeth Priddy

Beaufort, NC - USA
http://www.elizabethpriddy.com

__________________________________________________
Do You Yahoo!?
Tired of spam? Yahoo! Mail has the best spam protection around
http://mail.yahoo.com

Donna Kat on sat 28 apr 07


On Sat, 28 Apr 2007 14:25:49 -0700, Elizabeth Priddy
wrote:

>http://www.flickr.com/photos/7973282@N03/
>
>
>Wood kiln results from second firing of my
>small low (cone 7) wood kiln.
>
>Ash works low too. It may need a little glaze.
>
>The chamber on the kiln is 18x18x30 of usable space.
>
>It took 5 hours to get to cone 7.
>
>I will add a few pictures of the kiln itself later.
>
>
>Elizabeth Priddy
>

Very nice! How many bricks of what grade did you use? Thanks, Donna