Julie,
I can recommend spending the summer at the Peters Valley Craft Center
here in Pennsylvania. Wood firing sculptor, Jim Jansma, fires up the
Valleys Anagama at least twice each summer, plus they have a wonderful
two-chambered cone 11 wood/salt kiln they regularly fire in the summer.
If you are interested, I'll be glad to Email you the rest of the contact
info.