white crackle raku glaze recipe?

updated tue 30 apr 96

 

Zane Dmytruk on fri 26 apr 96

hello!

On behalf of a fellow potter, I'm requesting any recipes out there
for a white crackle raku glaze. I enjoy the Clayart line. Thanks, Jan

Jack Phillips on sun 28 apr 96

>----------------------------Original message----------------------------
> hello!
>
> On behalf of a fellow potter, I'm requesting any recipes out there
>for a white crackle raku glaze. I enjoy the Clayart line. Thanks, Jan
>
Jan,
There is a simple starting point for a clear raku crackle.

80% gerstley borate, 20% neph sy. To make white, add tin oxide from 2%
to 10%. Make a small batch, see how you like it.

Jack Phillips
STONART Ceramic art
Portland, Oregon