search  current discussion  categories  techniques - misc 

wax resist alternative

updated fri 31 may 96

 

Christine Fennimore on tue 7 may 96

I have experimented with fabric softner as a wax resist alternative in
the past with fair results. The pots should be glazed right away and not
left to sit too long as the fabric softner looses something over time.
You will still need to do a little cleaning off of the bottoms, but it's
much less expensive than wax resist.