Eleanora Eden on sun 9 feb 97

Hi All,

I find that if you apply wax out of a squeeze bottle you get such a nice
thick application that stuff tends to stick to it less and what does
stick to it is easier to remove by scraping with a knife and taking a bit
of the thick wax too.

About latex, I just pre-dip the DRY brush in any dish detergent and then
after using dip the brush again in the liquid detergent and rub all the
latex off before using water. No more wrecked brushes.

Cheers on a sunny Sunday morning.

Eleanora

Got my paperclay drying in pillowcases hanging from the rafters in my studio.
BTW I got my pulp from a local mill, enough to do a first batch.
Thankyou Clayarters for these tips. Will be using the paperclay for tiles.


Eleanora Eden 802 869-2003
Paradise Hill
Bellows Falls, VT 05101 eden@maple.sover.net

[the address fga@world.std.com is temporary. My mailbox at
eden@maple.sover.net still works -- do not change address books]