search  current discussion  categories  glazes - misc 

volcanic glazes

updated tue 30 sep 97

 

SUSAN MASTERMAN on thu 18 sep 97

Im looking for a gnarly volcanic high temperature glaze. Any help would be
much appreciated.

Susan Masterman

A.D. on fri 19 sep 97

Just and idea but go look for something on Mt. St helens.. I know lost of
people up here gather the ash from that and make some cool glazes.

At 07:00 AM 9/18/97 EDT, you wrote:
>----------------------------Original message----------------------------
>Im looking for a gnarly volcanic high temperature glaze. Any help would be
>much appreciated.
>
>Susan Masterman
>
>