search  current discussion  categories  techniques - stains 

underglaze formulas

updated sat 31 may 97

 

Thomas Orr on wed 30 apr 97

Here at OCAC, where Harris Deller is coming to do a workshop this weekend,
followed by Eva Kwong in June and Kirk Mangus in July, we use a C/6 casting
slip as a base and mason stains to color. Works well.

Thomas Orr
Department Head, Ceramics torr@teleport.com
Oregon College of Art and Craft (503) 297-5544 voice
Portland OR, 97225 (503) 297-9651 fax

Joyce Lee, Jim Lee on thu 1 may 97

Thomas Orr wrote:
>
> ----------------------------Original message----------------------------
> Here at OCAC, where Harris Deller is coming to do a workshop this weekend,
> followed by Eva Kwong in June and Kirk Mangus in July, we use a C/6 casting
> slip as a base and mason stains to color. Works well.
>
> Thomas Orr
> Department Head, Ceramics torr@teleport.com
> Oregon College of Art and Craft (503) 297-5544 voice
> Portland OR, 97225 (503) 297-9651 fax

\\Good morning Thomas,

Do you then use these underglazes on ^10 R work? Thanks for taking your
time to respond.

Joyce
Desert Rat