Linhares on tue 10 dec 96


Hellooo Clayart

I have heard of taking unwanted glaze material and firing it in the kiln.
Put the powder in a saggar or unwanted bisque bowl and fire it until it
turns into a glaze. If it is a scrap glaze from the studio sink trap it
most likely will fire to the same temp as your other glazes. Then take your
chunk of insoluable glass and bury it in the back yard if you want.

Paul in Ohio where it's snowing!!!