Perhaps this will help...We've raised the bisque temp. for all our clays
(especially the red ones) to ^02, with a firing time of appr. 12 hours.
This helped with a variety of glaze problems. I realize that this sounds
excessive, but it helped us quite a bit. We glaze to ^6. Good luck and
let us know what happens!