search  current discussion  categories  tools & equipment - slab rollers 

slab roller grit found

updated fri 31 jan 97

 

sam wainford on thu 9 jan 97

My local server has been down but I managed to retrieve replies to my
question from the clayart archives. Thanks to all for the ideas and
cautions.

For Karen's problem of recoating the board: the two part epoxy paint
from Sherwin Williams called Tile CladII with the Bondex additive should
work on the board as well as the roller. I have not tested my rollers
yet since I applied this stuff last Sunday. Takes a week to cure. I'll
write as soon as I test it on the results. If the grit wears off on
this, it'll be easy to recoat. It took about 20 minutes.

Sam