I recently was given an AIM kiln with a Sigma MPC10 controller. The
instruction manual is a nightmare to say the least. The previous owners were
unable to get it to operate with only one exception--luck, not skill. If
anyone out there has any experience with this model, please give me a clue
as to how to unravel this mess. Any feed back will be greatly appreciated.

TIA

Donald Goldsobel in the rainy San Fermando Valley where trying to dry
anything is becoming a challenge.