search  current discussion  categories  kilns & firing - bisque 

repair broke bisque

updated mon 30 sep 96

 

Kim Creeley on fri 27 sep 96

I'm not all that experienced, but I think its o.k. to glue the sculpture,
after you've Rakued. Also I've used Dispex, to repair bisque. Hope thats
some help!