search  current discussion  categories  glazes - misc 

reglaze report

updated sun 31 aug 97

 

P. F. S. on sun 17 aug 97

Awhile back I made this post:

"If I want to reglaze a pot with a glossy surface using the same glaze
again, what additive should I use to improve adherence of the glaze
for the second firing."

I wanted to reglaze the center of a lid. I ran hot water over the lid
and dabbed on some glaze sediment from the bottom of the bucket. I used
no additives. It worked. Thanks
again to all who made suggestions.