search  current discussion  categories  glazes - misc 

recipe question

updated wed 30 apr 97

 

Judith Enright on tue 15 apr 97

I pulled a recipe off the CeramicsWeb offered by Brian Kemp and have a
question before mixing it up. It's called IE76:

Very pale Pink:

Neph Sye 46.43
Whiting 21.43
Gerstley Borate 8.93
Lithium Carb 17.86
Barium Carb 5.36

ADD:

Silica (flint) 78.55
Tin Oxide 7.14
Rutile 5.36

I'm confused about the Silica -- can this possibly be right? Any
advice appreciated.

-- Judith Enright @ Black Leopard Clayware and Pottery -- getting just
a bit crazed readying for Open Studios next weekend!!

Robert Speirs, M.D. 766 X4450 on wed 16 apr 97

What cone is this Very Pale Pink glaze?

Laura in Oregon

KEMPB on thu 17 apr 97

Very Oale Oink glaze is a Cone 6/7 glaze

Brian Kemp. Singapore
kempb@nievax.nie.ac.sg