recipe format

updated wed 30 apr 97

 

Tony Hansen on sun 20 apr 97

A lot of recipes come across Clayart like this:

> Gerstley Borate 8.4
> Neph Sy 14
> Potash Feldspar 27
> Whiting 12

Why don't we do it like this with two spaces between material
and amount:

Gerstley Borate 8.4
Nepheline Syenite 14

Or like this:

8.4 Gerstley Borate
14.0 Nepheline Syenite

--